Back
|
Chemical Composition
Alloy No.
|
Cr
|
Si
|
Fe
|
Pb
|
Zr
|
Cu
|
C18200
|
0.6~1.2
|
≤ 0.1
|
≤ 0.1
|
≤ 0.05
|
|
Balance
|
C18150
|
0.5~1.5
|
≤ 0.1
|
|
|
0.5~0.25
|
Rem
|
|
Shape
|
Size
|
HRB
|
Conductivity(% IACS)
|
Tensile Strength
(kg/㎜²)
|
Rod
|
Ф2~Ф20
|
≥ 72
|
≥ 75%
|
≥ 42
|
Ф22~Ф40
|
≥ 72
|
≥ 75%
|
≥ 46
|
Ф45~Ф100
|
≥ 72
|
≥ 75%
|
≥ 46
|
Plate
|
0.1t~10t
|
≥ 72
|
≥ 75%
|
≥ 420
|
11t~30t
|
≥ 72
|
≥ 75%
|
≥ 42
|
32t~100t
|
≥ 72
|
≥ 75%
|
≥ 44
|
-
|
-
|
≥ 50
|
≥ 70%
|
≥ 38
|
It has 0.4% ~ 1.2% of Chrome and softening temperature and the electrical conductivity is high, and thermal
conductivity and excellent in strength.